The first castings!
The top casting is in UreCoat, the bottom is Task 14. The Task was much easier to cast, and is fairly flexible, however it's a little plastic-y. The UreCoat is much more flexible, but is more viscous, and the pot life is much shorter, so it's prone to air bubbles.